2011 Aluminum vs. 88-silver 12-tin-oxide
2011 aluminum belongs to the aluminum alloys classification, while 88-silver 12-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (24, in this case) are not shown.
For each property being compared, the top bar is 2011 aluminum and the bottom bar is 88-silver 12-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 35 to 45 | |
84 to 86 |
Elongation at Break, % | 8.5 to 18 | |
9.0 to 37 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 29 to 52 | |
24 to 70 |
Shear Strength, MPa | 190 to 250 | |
150 to 160 |
Tensile Strength: Ultimate (UTS), MPa | 310 to 420 | |
230 to 280 |
Tensile Strength: Yield (Proof), MPa | 140 to 310 | |
110 to 260 |