Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 4.1 | |
76 to 80 |
Elongation at Break, % | 1.1 to 28 | |
32 to 34 |
Shear Strength, MPa | 220 to 350 | |
150 to 210 |
Tensile Strength: Ultimate (UTS), MPa | 340 to 720 | |
230 to 320 |