60Pd-40Ag Alloy vs. Nuclear Grade Hafnium
Both 60Pd-40Ag alloy and nuclear grade hafnium are otherwise unclassified metals. There are 14 material properties with values for both materials. Properties with values for just one material (11, in this case) are not shown.
For each property being compared, the top bar is 60Pd-40Ag alloy and the bottom bar is nuclear grade hafnium.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 100 | |
78 |
Elongation at Break, % | 1.1 to 28 | |
25 |
Poisson's Ratio | 0.38 | |
0.26 |
Shear Modulus, GPa | 37 | |
31 |
Tensile Strength: Ultimate (UTS), MPa | 340 to 720 | |
350 |
Thermal Properties
Latent Heat of Fusion, J/g | 140 | |
130 |
Specific Heat Capacity, J/kg-K | 240 | |
140 |
Thermal Expansion, µm/m-K | 15 | |
5.9 |
Otherwise Unclassified Properties
Density, g/cm3 | 11 | |
13 |
Common Calculations
Stiffness to Weight: Axial, points | 4.9 | |
3.3 |
Stiffness to Weight: Bending, points | 14 | |
11 |
Strength to Weight: Axial, points | 8.4 to 18 | |
7.4 |
Strength to Weight: Bending, points | 9.6 to 16 | |
8.4 |
Thermal Shock Resistance, points | 16 to 34 | |
55 |
Alloy Composition
Copper (Cu), % | 0 to 0.1 | |
0 |
Hafnium (Hf), % | 0 | |
99.8 to 100 |
Palladium (Pd), % | 59.5 to 60.9 | |
0 |
Silver (Ag), % | 39.1 to 40.5 | |
0 |
Residuals, % | 0 | |
0 to 0.23 |