Metric UnitsUS Customary Units
Material Properties
Density, g/cm3 | 9.9 | |
7.8 |
Electrical Conductivity: Equal Volume, % IACS | 63 to 77 | |
7.3 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 57 to 70 | |
8.4 |
Elongation at Break, % | 1.1 to 15 | |
22 |
Shear Strength, MPa | 190 to 220 | |
340 |
Strength to Weight: Axial, points | 8.8 to 12 | |
19 |
Strength to Weight: Bending, points | 10 to 13 | |
19 |
Tensile Strength: Ultimate (UTS), MPa | 310 to 440 | |
540 |