Electrical Conductivity: Equal Volume, % IACS | 84 to 86 | |
40 |
Elongation at Break, % | 9.0 to 37 | |
5.0 to 5.7 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 24 to 70 | |
28 to 32 |
Shear Strength, MPa | 150 to 160 | |
340 to 350 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 280 | |
580 to 590 |
Tensile Strength: Yield (Proof), MPa | 110 to 260 | |
500 to 530 |