Electrical Conductivity: Equal Volume, % IACS 84 to 86
2.2
Elongation at Break, % 9.0 to 37
18
Resilience: Ultimate (Unit Rupture Work), MJ/m3 24 to 70
150
Tensile Strength: Ultimate (UTS), MPa 230 to 280
880
Tensile Strength: Yield (Proof), MPa 110 to 260