88-silver 12-tin-oxide vs. ASTM B477 Au-Ni-Ag
Both 88-silver 12-tin-oxide and ASTM B477 Au-Ni-Ag are otherwise unclassified metals. There are 4 material properties with values for both materials. Properties with values for just one material (18, in this case) are not shown.
For each property being compared, the top bar is 88-silver 12-tin-oxide and the bottom bar is ASTM B477 Au-Ni-Ag.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 84 to 86 | |
14 |
Elongation at Break, % | 9.0 to 37 | |
5.5 to 11 |
Shear Strength, MPa | 150 to 160 | |
190 to 320 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 280 | |
310 to 550 |