88-silver 12-tin-oxide vs. Solder Alloy 801
Both 88-silver 12-tin-oxide and solder alloy 801 are otherwise unclassified metals. There are 3 material properties with values for both materials. Properties with values for just one material (24, in this case) are not shown.
For each property being compared, the top bar is 88-silver 12-tin-oxide and the bottom bar is solder alloy 801.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 84 to 86 | |
15 |
Elongation at Break, % | 9.0 to 37 | |
33 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 280 | |
55 |