88-silver 12-tin-oxide vs. SAE-AISI 4615 Steel

88-silver 12-tin-oxide belongs to the otherwise unclassified metals classification, while SAE-AISI 4615 steel belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (25, in this case) are not shown.

For each property being compared, the top bar is 88-silver 12-tin-oxide and the bottom bar is SAE-AISI 4615 steel.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 84 to 86
7.3
Elongation at Break, % 9.0 to 37
27
Resilience: Ultimate (Unit Rupture Work), MJ/m3 24 to 70
120
Shear Strength, MPa 150 to 160
310
Tensile Strength: Ultimate (UTS), MPa 230 to 280
480
Tensile Strength: Yield (Proof), MPa 110 to 260
350