90-silver 10-tin-oxide vs. AISI 316N Stainless Steel
90-silver 10-tin-oxide belongs to the otherwise unclassified metals classification, while AISI 316N stainless steel belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (27, in this case) are not shown.
For each property being compared, the top bar is 90-silver 10-tin-oxide and the bottom bar is AISI 316N stainless steel.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 77 to 82 | |
2.3 |
Elongation at Break, % | 7.0 to 35 | |
9.0 to 39 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 20 to 68 | |
95 to 230 |
Shear Strength, MPa | 160 to 170 | |
420 to 690 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 300 | |
620 to 1160 |
Tensile Strength: Yield (Proof), MPa | 120 to 280 | |
270 to 870 |