90-silver 10-tin-oxide vs. K94200 Alloy
90-silver 10-tin-oxide belongs to the otherwise unclassified metals classification, while K94200 alloy belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is 90-silver 10-tin-oxide and the bottom bar is K94200 alloy.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 77 to 82 | |
2.7 |
Elongation at Break, % | 7.0 to 35 | |
5.0 to 32 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 20 to 68 | |
35 to 130 |
Shear Strength, MPa | 160 to 170 | |
330 to 410 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 300 | |
500 to 710 |
Tensile Strength: Yield (Proof), MPa | 120 to 280 | |
270 to 650 |