Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
6.2 |
Elongation at Break, % | 32 to 34 | |
5.5 to 34 |
Shear Strength, MPa | 150 to 210 | |
370 to 420 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
560 to 730 |