MakeItFrom.com
Menu (ESC)

92-silver 8-tin-oxide vs. ACI-ASTM CA6N Steel

92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while ACI-ASTM CA6N steel belongs to the iron alloys. There are 5 material properties with values for both materials. Properties with values for just one material (28, in this case) are not shown.

For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is ACI-ASTM CA6N steel.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 76 to 80
2.6
Elongation at Break, % 32 to 34
17
Resilience: Ultimate (Unit Rupture Work), MJ/m3 62 to 110
180
Tensile Strength: Ultimate (UTS), MPa 230 to 320
1080
Tensile Strength: Yield (Proof), MPa 120 to 300
1060