92-silver 8-tin-oxide vs. ACI-ASTM CB7Cu-2 Steel
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while ACI-ASTM CB7Cu-2 steel belongs to the iron alloys. There are 5 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is ACI-ASTM CB7Cu-2 steel.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
2.1 |
Elongation at Break, % | 32 to 34 | |
5.7 to 11 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
71 to 120 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
960 to 1350 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
760 to 1180 |