MakeItFrom.com
Menu (ESC)

92-silver 8-tin-oxide vs. AISI 301LN Stainless Steel

92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while AISI 301LN stainless steel belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (27, in this case) are not shown.

For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is AISI 301LN stainless steel.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 76 to 80
2.4
Elongation at Break, % 32 to 34
23 to 51
Resilience: Ultimate (Unit Rupture Work), MJ/m3 62 to 110
220 to 290
Shear Strength, MPa 150 to 210
450 to 670
Tensile Strength: Ultimate (UTS), MPa 230 to 320
630 to 1060
Tensile Strength: Yield (Proof), MPa 120 to 300
270 to 770