92-silver 8-tin-oxide vs. AISI 410Cb Stainless Steel
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while AISI 410Cb stainless steel belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (28, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is AISI 410Cb stainless steel.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
2.9 |
Elongation at Break, % | 32 to 34 | |
15 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
70 to 130 |
Shear Strength, MPa | 150 to 210 | |
340 to 590 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
550 to 960 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
310 to 790 |