92-silver 8-tin-oxide vs. ASTM A182 Grade F12 Class 2
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while ASTM A182 grade F12 class 2 belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (27, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is ASTM A182 grade F12 class 2.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
7.3 |
Elongation at Break, % | 32 to 34 | |
22 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
100 |
Shear Strength, MPa | 150 to 210 | |
340 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
540 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
310 |