92-silver 8-tin-oxide vs. ASTM A229 Spring Steel
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while ASTM A229 spring steel belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (25, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is ASTM A229 spring steel.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
7.2 |
Elongation at Break, % | 32 to 34 | |
14 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
200 to 230 |
Shear Strength, MPa | 150 to 210 | |
1020 to 1140 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
1690 to 1890 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
1100 to 1230 |