92-silver 8-tin-oxide vs. ASTM A302 Alloy Steel
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while ASTM A302 alloy steel belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (25, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is ASTM A302 alloy steel.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
7.2 to 7.4 |
Elongation at Break, % | 32 to 34 | |
20 to 23 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
110 to 120 |
Shear Strength, MPa | 150 to 210 | |
370 to 390 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
590 to 620 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
350 to 390 |