92-silver 8-tin-oxide vs. ASTM B540 Palladium
Both 92-silver 8-tin-oxide and ASTM B540 palladium are otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (18, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is ASTM B540 palladium.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
4.9 to 5.5 |
Elongation at Break, % | 32 to 34 | |
1.1 to 14 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
13 to 100 |
Shear Strength, MPa | 150 to 210 | |
500 to 700 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
830 to 1240 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
620 to 1000 |