92-silver 8-tin-oxide vs. EN AC-48000 Aluminum
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while EN AC-48000 aluminum belongs to the aluminum alloys. There are 5 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is EN AC-48000 aluminum.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
33 |
Elongation at Break, % | 32 to 34 | |
1.0 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
2.2 to 3.0 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
220 to 310 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
210 to 270 |