MakeItFrom.com
Menu (ESC)

92-silver 8-tin-oxide vs. Solder Alloy 301

Both 92-silver 8-tin-oxide and solder alloy 301 are otherwise unclassified metals. There are 5 material properties with values for both materials. Properties with values for just one material (22, in this case) are not shown.

For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is solder alloy 301.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 76 to 80
4.7
Elongation at Break, % 32 to 34
51
Resilience: Ultimate (Unit Rupture Work), MJ/m3 62 to 110
27
Tensile Strength: Ultimate (UTS), MPa 230 to 320
55
Tensile Strength: Yield (Proof), MPa 120 to 300
49