92-silver 8-tin-oxide vs. SAE-AISI 1108 Steel
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while SAE-AISI 1108 steel belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (26, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is SAE-AISI 1108 steel.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
7.0 |
Elongation at Break, % | 32 to 34 | |
23 to 34 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
95 to 110 |
Shear Strength, MPa | 150 to 210 | |
250 to 280 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
380 to 440 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
220 to 360 |