Electrical Conductivity: Equal Volume, % IACS 76 to 80
7.1
Elongation at Break, % 32 to 34
17 to 26
Resilience: Ultimate (Unit Rupture Work), MJ/m3 62 to 110
86 to 110
Shear Strength, MPa 150 to 210
320 to 330
Tensile Strength: Ultimate (UTS), MPa 230 to 320
490 to 540
Tensile Strength: Yield (Proof), MPa 120 to 300
260 to 460