Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
7.2 |
Elongation at Break, % | 32 to 34 | |
13 to 26 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
83 to 180 |
Shear Strength, MPa | 150 to 210 | |
340 to 640 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
530 to 1040 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
440 to 980 |