92-silver 8-tin-oxide vs. K93600 Alloy
92-silver 8-tin-oxide belongs to the otherwise unclassified metals classification, while K93600 alloy belongs to the iron alloys. There are 6 material properties with values for both materials. Properties with values for just one material (16, in this case) are not shown.
For each property being compared, the top bar is 92-silver 8-tin-oxide and the bottom bar is K93600 alloy.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 76 to 80 | |
2.2 |
Elongation at Break, % | 32 to 34 | |
5.0 to 35 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 62 to 110 | |
21 to 280 |
Shear Strength, MPa | 150 to 210 | |
320 to 380 |
Tensile Strength: Ultimate (UTS), MPa | 230 to 320 | |
480 to 810 |
Tensile Strength: Yield (Proof), MPa | 120 to 300 | |
280 to 750 |