Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 76 to 80
2.7
Elongation at Break, % 32 to 34
5.0 to 32
Resilience: Ultimate (Unit Rupture Work), MJ/m3 62 to 110
35 to 130
Shear Strength, MPa 150 to 210
330 to 410
Tensile Strength: Ultimate (UTS), MPa 230 to 320
500 to 710
Tensile Strength: Yield (Proof), MPa 120 to 300
270 to 650