MakeItFrom.com
Menu (ESC)

ACI-ASTM CA6NM Steel vs. 88-silver 12-tin-oxide

ACI-ASTM CA6NM steel belongs to the iron alloys classification, while 88-silver 12-tin-oxide belongs to the otherwise unclassified metals. There are 5 material properties with values for both materials. Properties with values for just one material (29, in this case) are not shown.

For each property being compared, the top bar is ACI-ASTM CA6NM steel and the bottom bar is 88-silver 12-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 2.8
84 to 86
Elongation at Break, % 17
9.0 to 37
Resilience: Ultimate (Unit Rupture Work), MJ/m3 130
24 to 70
Tensile Strength: Ultimate (UTS), MPa 850
230 to 280
Tensile Strength: Yield (Proof), MPa 620
110 to 260