Electrical Conductivity: Equal Volume, % IACS 2.1
84 to 86
Elongation at Break, % 28
9.0 to 37
Resilience: Ultimate (Unit Rupture Work), MJ/m3 180
24 to 70
Tensile Strength: Ultimate (UTS), MPa 730
230 to 280
Tensile Strength: Yield (Proof), MPa 510
110 to 260