ACI-ASTM CG3M steel belongs to the iron alloys classification, while 92-silver 8-tin-oxide belongs to the otherwise unclassified metals. There are 5 material properties with values for both materials. Properties with values for just one material (28, in this case) are not shown.

For each property being compared, the top bar is ACI-ASTM CG3M steel and the bottom bar is 92-silver 8-tin-oxide.

Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 2.0
76 to 80
Elongation at Break, % 28
32 to 34
Resilience: Ultimate (Unit Rupture Work), MJ/m3 130
62 to 110
Tensile Strength: Ultimate (UTS), MPa 580
230 to 320
Tensile Strength: Yield (Proof), MPa 270
120 to 300