AISI 410Cb Stainless Steel vs. 88-silver 12-tin-oxide
AISI 410Cb stainless steel belongs to the iron alloys classification, while 88-silver 12-tin-oxide belongs to the otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (28, in this case) are not shown.
For each property being compared, the top bar is AISI 410Cb stainless steel and the bottom bar is 88-silver 12-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 2.9 | |
84 to 86 |
Elongation at Break, % | 15 | |
9.0 to 37 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 70 to 130 | |
24 to 70 |
Shear Strength, MPa | 340 to 590 | |
150 to 160 |
Tensile Strength: Ultimate (UTS), MPa | 550 to 960 | |
230 to 280 |
Tensile Strength: Yield (Proof), MPa | 310 to 790 | |
110 to 260 |