Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 17 to 18 | |
5.0 to 16 |
Fatigue Strength, MPa | 240 | |
310 to 860 |
Poisson's Ratio | 0.29 | |
0.28 |
Shear Modulus, GPa | 73 | |
75 |
Shear Strength, MPa | 360 to 410 | |
460 to 1160 |
Tensile Strength: Ultimate (UTS), MPa | 590 to 670 | |
760 to 2000 |
Tensile Strength: Yield (Proof), MPa | 350 to 360 | |
470 to 1510 |
Thermal Properties
Latent Heat of Fusion, J/g | 260 | |
270 |
Melting Completion (Liquidus), °C | 1450 | |
1440 |
Melting Onset (Solidus), °C | 1410 | |
1390 |
Specific Heat Capacity, J/kg-K | 470 | |
480 |
Thermal Conductivity, W/m-K | 52 | |
31 |
Thermal Expansion, µm/m-K | 13 | |
11 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.3 | |
4.3 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.4 | |
5.1 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 2.1 | |
8.0 |
Density, g/cm3 | 7.8 | |
7.7 |
Embodied Carbon, kg CO2/kg material | 1.4 | |
3.4 |
Embodied Energy, MJ/kg | 19 | |
50 |
Embodied Water, L/kg | 49 | |
100 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 93 to 96 | |
92 to 100 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 330 to 350 | |
570 to 5940 |
Stiffness to Weight: Axial, points | 13 | |
14 |
Stiffness to Weight: Bending, points | 24 | |
25 |
Strength to Weight: Axial, points | 21 to 24 | |
27 to 72 |
Strength to Weight: Bending, points | 20 to 22 | |
24 to 46 |
Thermal Diffusivity, mm2/s | 14 | |
8.3 |
Thermal Shock Resistance, points | 17 to 20 | |
25 to 67 |