Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
110
Elongation at Break, % 17 to 18
43
Poisson's Ratio 0.29
0.31
Shear Modulus, GPa 73
39
Shear Strength, MPa 360 to 410
240
Tensile Strength: Ultimate (UTS), MPa 590 to 670
350
Tensile Strength: Yield (Proof), MPa 350 to 360
120

Thermal Properties

Latent Heat of Fusion, J/g 260
180
Maximum Temperature: Mechanical, °C 410
140
Melting Completion (Liquidus), °C 1450
930
Melting Onset (Solidus), °C 1410
910
Specific Heat Capacity, J/kg-K 470
390
Thermal Conductivity, W/m-K 52
120
Thermal Expansion, µm/m-K 13
20

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.3
26
Electrical Conductivity: Equal Weight (Specific), % IACS 8.4
29

Otherwise Unclassified Properties

Base Metal Price, % relative 2.1
25
Density, g/cm3 7.8
8.2
Embodied Carbon, kg CO2/kg material 1.4
2.9
Embodied Energy, MJ/kg 19
48
Embodied Water, L/kg 49
320

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 93 to 96
120
Resilience: Unit (Modulus of Resilience), kJ/m3 330 to 350
63
Stiffness to Weight: Axial, points 13
7.4
Stiffness to Weight: Bending, points 24
19
Strength to Weight: Axial, points 21 to 24
12
Strength to Weight: Bending, points 20 to 22
14
Thermal Diffusivity, mm2/s 14
37
Thermal Shock Resistance, points 17 to 20
12