Brinell Hardness | 160 to 180 | |
130 to 140 |
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 22 to 26 | |
6.7 to 24 |
Fatigue Strength, MPa | 210 to 280 | |
170 to 220 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
73 |
Shear Strength, MPa | 330 to 370 | |
280 to 290 |
Tensile Strength: Ultimate (UTS), MPa | 520 to 590 | |
440 to 500 |
Tensile Strength: Yield (Proof), MPa | 290 to 390 | |
230 to 380 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
250 |
Maximum Temperature: Mechanical, °C | 410 | |
400 |
Melting Completion (Liquidus), °C | 1460 | |
1460 |
Melting Onset (Solidus), °C | 1420 | |
1420 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 52 | |
52 |
Thermal Expansion, µm/m-K | 13 | |
12 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.4 to 7.6 | |
7.1 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.5 to 8.7 | |
8.1 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 3.2 to 4.0 | |
1.8 |
Density, g/cm3 | 7.9 | |
7.8 |
Embodied Carbon, kg CO2/kg material | 1.6 to 1.7 | |
1.4 |
Embodied Energy, MJ/kg | 21 to 23 | |
18 |
Embodied Water, L/kg | 50 to 52 | |
46 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 110 to 120 | |
31 to 95 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 230 to 410 | |
140 to 390 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 18 to 21 | |
16 to 18 |
Strength to Weight: Bending, points | 18 to 20 | |
16 to 18 |
Thermal Diffusivity, mm2/s | 14 | |
14 |
Thermal Shock Resistance, points | 15 to 17 | |
14 to 16 |