ASTM A209 Steel vs. AWS E2595
Both ASTM A209 steel and AWS E2595 are iron alloys. There are 24 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown.
For each property being compared, the top bar is ASTM A209 steel and the bottom bar is AWS E2595.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
200 |
Elongation at Break, % | 34 | |
17 |
Poisson's Ratio | 0.29 | |
0.27 |
Shear Modulus, GPa | 73 | |
80 |
Tensile Strength: Ultimate (UTS), MPa | 420 to 460 | |
850 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
300 |
Melting Completion (Liquidus), °C | 1470 | |
1450 |
Melting Onset (Solidus), °C | 1420 to 1430 | |
1400 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 50 | |
16 |
Thermal Expansion, µm/m-K | 13 | |
14 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.1 | |
2.2 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.1 to 8.2 | |
2.5 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 2.4 | |
23 |
Density, g/cm3 | 7.9 | |
7.9 |
Embodied Carbon, kg CO2/kg material | 1.5 | |
4.4 |
Embodied Energy, MJ/kg | 20 | |
61 |
Embodied Water, L/kg | 47 | |
190 |
Common Calculations
Stiffness to Weight: Axial, points | 13 | |
14 |
Stiffness to Weight: Bending, points | 24 | |
25 |
Strength to Weight: Axial, points | 15 to 16 | |
30 |
Strength to Weight: Bending, points | 16 to 17 | |
25 |
Thermal Diffusivity, mm2/s | 13 | |
4.2 |
Thermal Shock Resistance, points | 12 to 14 | |
21 |