Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
210 to 250
Elongation at Break, % 34
12
Fatigue Strength, MPa 180 to 200
250 to 840
Poisson's Ratio 0.29
0.29
Shear Modulus, GPa 73
82 to 98
Tensile Strength: Ultimate (UTS), MPa 420 to 460
780 to 1280
Tensile Strength: Yield (Proof), MPa 220 to 250
480 to 840

Thermal Properties

Latent Heat of Fusion, J/g 250
320
Melting Completion (Liquidus), °C 1470
1360
Melting Onset (Solidus), °C 1420 to 1430
1290
Specific Heat Capacity, J/kg-K 470
450
Thermal Conductivity, W/m-K 50
13
Thermal Expansion, µm/m-K 13
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.1
2.0
Electrical Conductivity: Equal Weight (Specific), % IACS 8.1 to 8.2
2.1

Otherwise Unclassified Properties

Density, g/cm3 7.9
8.4
Embodied Carbon, kg CO2/kg material 1.5
8.1
Embodied Energy, MJ/kg 20
110
Embodied Water, L/kg 47
530

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 120 to 130
84 to 140
Resilience: Unit (Modulus of Resilience), kJ/m3 130 to 170
560 to 1410
Stiffness to Weight: Axial, points 13
14 to 17
Stiffness to Weight: Bending, points 24
24 to 25
Strength to Weight: Axial, points 15 to 16
26 to 42
Strength to Weight: Bending, points 16 to 17
22 to 31
Thermal Diffusivity, mm2/s 13
3.5
Thermal Shock Resistance, points 12 to 14
21 to 29