MakeItFrom.com
Menu (ESC)

ASTM A225 Steel vs. ASTM A229 Spring Steel

Both ASTM A225 steel and ASTM A229 spring steel are iron alloys.

For each property being compared, the top bar is ASTM A225 steel and the bottom bar is ASTM A229 spring steel.

Metric UnitsUS Customary Units

Mechanical Properties

Brinell Hardness 190 to 250
490 to 550
Elastic (Young's, Tensile) Modulus, GPa 190
190
Elongation at Break, % 21 to 23
14
Fatigue Strength, MPa 330 to 390
710 to 790
Poisson's Ratio 0.29
0.29
Shear Modulus, GPa 73
72
Shear Strength, MPa 390 to 520
1020 to 1140
Tensile Strength: Ultimate (UTS), MPa 620 to 830
1690 to 1890
Tensile Strength: Yield (Proof), MPa 460 to 550
1100 to 1230

Thermal Properties

Latent Heat of Fusion, J/g 250
250
Maximum Temperature: Mechanical, °C 400
400
Melting Completion (Liquidus), °C 1460
1450
Melting Onset (Solidus), °C 1420
1410
Specific Heat Capacity, J/kg-K 470
470
Thermal Conductivity, W/m-K 52
50
Thermal Expansion, µm/m-K 13
12

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.3
7.2
Electrical Conductivity: Equal Weight (Specific), % IACS 8.4
8.3

Otherwise Unclassified Properties

Base Metal Price, % relative 2.3
1.8
Density, g/cm3 7.8
7.8
Embodied Carbon, kg CO2/kg material 1.8
1.4
Embodied Energy, MJ/kg 24 to 25
19
Embodied Water, L/kg 48
46

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 120 to 170
200 to 230
Resilience: Unit (Modulus of Resilience), kJ/m3 580 to 820
3260 to 4080
Stiffness to Weight: Axial, points 13
13
Stiffness to Weight: Bending, points 24
24
Strength to Weight: Axial, points 22 to 29
60 to 67
Strength to Weight: Bending, points 21 to 25
40 to 43
Thermal Diffusivity, mm2/s 14
14
Thermal Shock Resistance, points 18 to 24
54 to 60

Comparable Variants