Metric UnitsUS Customary Units

Material Properties

Electrical Conductivity: Equal Volume, % IACS 7.3
84 to 86
Elongation at Break, % 14
9.0 to 37
Resilience: Ultimate (Unit Rupture Work), MJ/m3 250
24 to 70
Shear Strength, MPa 1090
150 to 160
Tensile Strength: Ultimate (UTS), MPa 1790
230 to 280
Tensile Strength: Yield (Proof), MPa 1610
110 to 260