MakeItFrom.com
Menu (ESC)

ASTM A27 Cast Steel vs. C82500 Copper

ASTM A27 cast steel belongs to the iron alloys classification, while C82500 copper belongs to the copper alloys. There are 27 material properties with values for both materials. Properties with values for just one material (3, in this case) are not shown.

For each property being compared, the top bar is ASTM A27 cast steel and the bottom bar is C82500 copper.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
120
Elongation at Break, % 25 to 27
1.0 to 20
Poisson's Ratio 0.29
0.33
Shear Modulus, GPa 73
45
Tensile Strength: Ultimate (UTS), MPa 460 to 550
550 to 1100
Tensile Strength: Yield (Proof), MPa 230 to 310
310 to 980

Thermal Properties

Latent Heat of Fusion, J/g 250
240
Maximum Temperature: Mechanical, °C 400
280
Melting Completion (Liquidus), °C 1460
980
Melting Onset (Solidus), °C 1420
860
Specific Heat Capacity, J/kg-K 470
390
Thermal Conductivity, W/m-K 52
130
Thermal Expansion, µm/m-K 12
17

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.0 to 7.1
20
Electrical Conductivity: Equal Weight (Specific), % IACS 8.1
21

Otherwise Unclassified Properties

Density, g/cm3 7.8
8.8
Embodied Carbon, kg CO2/kg material 1.4
10
Embodied Energy, MJ/kg 18
160
Embodied Water, L/kg 45 to 46
310

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 96 to 120
11 to 94
Resilience: Unit (Modulus of Resilience), kJ/m3 140 to 260
400 to 4000
Stiffness to Weight: Axial, points 13
7.7
Stiffness to Weight: Bending, points 24
19
Strength to Weight: Axial, points 16 to 20
18 to 35
Strength to Weight: Bending, points 17 to 19
17 to 27
Thermal Diffusivity, mm2/s 14
38
Thermal Shock Resistance, points 15 to 18
19 to 38