ASTM A283 Carbon Steel vs. EN 1.7216 Steel
Both ASTM A283 carbon steel and EN 1.7216 steel are iron alloys.
For each property being compared, the top bar is ASTM A283 carbon steel and the bottom bar is EN 1.7216 steel.
Metric UnitsUS Customary Units
Mechanical Properties
Brinell Hardness | 110 to 140 | |
200 to 280 |
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 26 to 34 | |
12 to 23 |
Fatigue Strength, MPa | 150 to 190 | |
290 to 440 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
73 |
Shear Strength, MPa | 240 to 310 | |
410 to 560 |
Tensile Strength: Ultimate (UTS), MPa | 360 to 480 | |
650 to 930 |
Tensile Strength: Yield (Proof), MPa | 180 to 260 | |
400 to 690 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
250 |
Maximum Temperature: Mechanical, °C | 400 | |
420 |
Melting Completion (Liquidus), °C | 1460 | |
1460 |
Melting Onset (Solidus), °C | 1420 | |
1420 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 51 to 53 | |
46 |
Thermal Expansion, µm/m-K | 12 | |
13 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.1 | |
7.2 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.1 | |
8.3 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 1.8 | |
2.4 |
Density, g/cm3 | 7.8 to 7.9 | |
7.8 |
Embodied Carbon, kg CO2/kg material | 1.4 | |
1.5 |
Embodied Energy, MJ/kg | 18 | |
20 |
Embodied Water, L/kg | 46 | |
50 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 100 to 110 | |
110 to 130 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 91 to 180 | |
430 to 1280 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 13 to 17 | |
23 to 33 |
Strength to Weight: Bending, points | 14 to 17 | |
21 to 27 |
Thermal Diffusivity, mm2/s | 14 | |
12 |
Thermal Shock Resistance, points | 11 to 15 | |
19 to 27 |