ASTM A283 Carbon Steel vs. R31538 Cobalt
ASTM A283 carbon steel belongs to the iron alloys classification, while R31538 cobalt belongs to the cobalt alloys. There are 27 material properties with values for both materials. Properties with values for just one material (6, in this case) are not shown.
For each property being compared, the top bar is ASTM A283 carbon steel and the bottom bar is R31538 cobalt.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
220 |
Elongation at Break, % | 26 to 34 | |
13 to 23 |
Fatigue Strength, MPa | 150 to 190 | |
310 to 480 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
86 |
Tensile Strength: Ultimate (UTS), MPa | 360 to 480 | |
1020 to 1360 |
Tensile Strength: Yield (Proof), MPa | 180 to 260 | |
580 to 930 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
320 |
Melting Completion (Liquidus), °C | 1460 | |
1360 |
Melting Onset (Solidus), °C | 1420 | |
1290 |
Specific Heat Capacity, J/kg-K | 470 | |
450 |
Thermal Conductivity, W/m-K | 51 to 53 | |
13 |
Thermal Expansion, µm/m-K | 12 | |
13 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.1 | |
2.0 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.1 | |
2.1 |
Otherwise Unclassified Properties
Density, g/cm3 | 7.8 to 7.9 | |
8.4 |
Embodied Carbon, kg CO2/kg material | 1.4 | |
8.1 |
Embodied Energy, MJ/kg | 18 | |
110 |
Embodied Water, L/kg | 46 | |
530 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 100 to 110 | |
140 to 200 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 91 to 180 | |
750 to 1920 |
Stiffness to Weight: Axial, points | 13 | |
15 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 13 to 17 | |
34 to 45 |
Strength to Weight: Bending, points | 14 to 17 | |
27 to 32 |
Thermal Diffusivity, mm2/s | 14 | |
3.5 |
Thermal Shock Resistance, points | 11 to 15 | |
25 to 33 |