ASTM A285 Carbon Steel vs. EN 1.1221 Steel
Both ASTM A285 carbon steel and EN 1.1221 steel are iron alloys.
For each property being compared, the top bar is ASTM A285 carbon steel and the bottom bar is EN 1.1221 steel.
Metric UnitsUS Customary Units
Mechanical Properties
Brinell Hardness | 110 to 130 | |
210 to 250 |
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 30 to 34 | |
10 to 21 |
Fatigue Strength, MPa | 150 to 180 | |
240 to 340 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
72 |
Shear Strength, MPa | 250 to 290 | |
450 to 520 |
Tensile Strength: Ultimate (UTS), MPa | 380 to 450 | |
730 to 870 |
Tensile Strength: Yield (Proof), MPa | 190 to 230 | |
390 to 550 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
250 |
Maximum Temperature: Mechanical, °C | 400 | |
400 |
Melting Completion (Liquidus), °C | 1470 | |
1460 |
Melting Onset (Solidus), °C | 1420 to 1430 | |
1410 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 53 | |
48 |
Thermal Expansion, µm/m-K | 12 | |
12 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.0 | |
7.2 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.0 | |
8.3 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 1.8 | |
2.1 |
Density, g/cm3 | 7.9 | |
7.8 |
Embodied Carbon, kg CO2/kg material | 1.4 | |
1.5 |
Embodied Energy, MJ/kg | 18 | |
19 |
Embodied Water, L/kg | 46 | |
47 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 110 | |
67 to 130 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 94 to 150 | |
410 to 800 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 13 to 16 | |
26 to 31 |
Strength to Weight: Bending, points | 15 to 17 | |
23 to 26 |
Thermal Diffusivity, mm2/s | 14 | |
13 |
Thermal Shock Resistance, points | 12 to 14 | |
23 to 28 |