ASTM A285 Carbon Steel vs. SAE-AISI 50B60 Steel
Both ASTM A285 carbon steel and SAE-AISI 50B60 steel are iron alloys.
For each property being compared, the top bar is ASTM A285 carbon steel and the bottom bar is SAE-AISI 50B60 steel.
Metric UnitsUS Customary Units
Mechanical Properties
Brinell Hardness | 110 to 130 | |
180 to 190 |
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 30 to 34 | |
12 to 20 |
Fatigue Strength, MPa | 150 to 180 | |
240 to 330 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
72 |
Shear Strength, MPa | 250 to 290 | |
380 |
Tensile Strength: Ultimate (UTS), MPa | 380 to 450 | |
610 to 630 |
Tensile Strength: Yield (Proof), MPa | 190 to 230 | |
350 to 530 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
250 |
Maximum Temperature: Mechanical, °C | 400 | |
410 |
Melting Completion (Liquidus), °C | 1470 | |
1450 |
Melting Onset (Solidus), °C | 1420 to 1430 | |
1410 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 53 | |
45 |
Thermal Expansion, µm/m-K | 12 | |
12 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.0 | |
7.2 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.0 | |
8.3 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 1.8 | |
2.0 |
Density, g/cm3 | 7.9 | |
7.8 |
Embodied Carbon, kg CO2/kg material | 1.4 | |
1.4 |
Embodied Energy, MJ/kg | 18 | |
19 |
Embodied Water, L/kg | 46 | |
48 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 110 | |
71 to 100 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 94 to 150 | |
330 to 750 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 13 to 16 | |
22 to 23 |
Strength to Weight: Bending, points | 15 to 17 | |
20 to 21 |
Thermal Diffusivity, mm2/s | 14 | |
12 |
Thermal Shock Resistance, points | 12 to 14 | |
20 |