ASTM A302 Alloy Steel vs. AWS ER80S-B2
Both ASTM A302 alloy steel and AWS ER80S-B2 are iron alloys. There are 27 material properties with values for both materials. Properties with values for just one material (5, in this case) are not shown.
For each property being compared, the top bar is ASTM A302 alloy steel and the bottom bar is AWS ER80S-B2.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
190 |
Elongation at Break, % | 20 to 23 | |
21 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
73 |
Tensile Strength: Ultimate (UTS), MPa | 590 to 620 | |
620 |
Tensile Strength: Yield (Proof), MPa | 350 to 390 | |
540 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
260 |
Melting Completion (Liquidus), °C | 1460 | |
1460 |
Melting Onset (Solidus), °C | 1420 | |
1420 |
Specific Heat Capacity, J/kg-K | 470 | |
470 |
Thermal Conductivity, W/m-K | 39 to 51 | |
40 |
Thermal Expansion, µm/m-K | 13 | |
13 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 7.2 to 7.4 | |
7.5 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 8.2 to 8.4 | |
8.6 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 2.4 to 3.0 | |
3.0 |
Density, g/cm3 | 7.8 to 7.9 | |
7.8 |
Embodied Carbon, kg CO2/kg material | 1.5 to 1.6 | |
1.6 |
Embodied Energy, MJ/kg | 20 to 21 | |
21 |
Embodied Water, L/kg | 48 to 50 | |
54 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 110 to 120 | |
130 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 330 to 410 | |
760 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 21 to 22 | |
22 |
Strength to Weight: Bending, points | 20 to 21 | |
21 |
Thermal Diffusivity, mm2/s | 10 to 14 | |
11 |
Thermal Shock Resistance, points | 17 to 18 | |
18 |