ASTM A302 Alloy Steel vs. EN 2.4878 Nickel
ASTM A302 alloy steel belongs to the iron alloys classification, while EN 2.4878 nickel belongs to the nickel alloys. There are 28 material properties with values for both materials. Properties with values for just one material (3, in this case) are not shown.
For each property being compared, the top bar is ASTM A302 alloy steel and the bottom bar is EN 2.4878 nickel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 190 | |
200 |
Elongation at Break, % | 20 to 23 | |
13 to 17 |
Fatigue Strength, MPa | 250 to 280 | |
400 to 410 |
Poisson's Ratio | 0.29 | |
0.29 |
Shear Modulus, GPa | 73 | |
78 |
Shear Strength, MPa | 370 to 390 | |
750 to 760 |
Tensile Strength: Ultimate (UTS), MPa | 590 to 620 | |
1210 to 1250 |
Tensile Strength: Yield (Proof), MPa | 350 to 390 | |
740 to 780 |
Thermal Properties
Latent Heat of Fusion, J/g | 250 | |
330 |
Maximum Temperature: Mechanical, °C | 410 | |
1030 |
Melting Completion (Liquidus), °C | 1460 | |
1370 |
Melting Onset (Solidus), °C | 1420 | |
1320 |
Specific Heat Capacity, J/kg-K | 470 | |
460 |
Thermal Conductivity, W/m-K | 39 to 51 | |
11 |
Thermal Expansion, µm/m-K | 13 | |
12 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 2.4 to 3.0 | |
80 |
Density, g/cm3 | 7.8 to 7.9 | |
8.3 |
Embodied Carbon, kg CO2/kg material | 1.5 to 1.6 | |
10 |
Embodied Energy, MJ/kg | 20 to 21 | |
150 |
Embodied Water, L/kg | 48 to 50 | |
370 |
Common Calculations
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 110 to 120 | |
150 to 180 |
Resilience: Unit (Modulus of Resilience), kJ/m3 | 330 to 410 | |
1370 to 1540 |
Stiffness to Weight: Axial, points | 13 | |
13 |
Stiffness to Weight: Bending, points | 24 | |
24 |
Strength to Weight: Axial, points | 21 to 22 | |
41 to 42 |
Strength to Weight: Bending, points | 20 to 21 | |
31 |
Thermal Diffusivity, mm2/s | 10 to 14 | |
2.8 |
Thermal Shock Resistance, points | 17 to 18 | |
37 to 39 |