ASTM A572 steel belongs to the iron alloys classification, while C97800 nickel silver belongs to the copper alloys. There are 28 material properties with values for both materials. Properties with values for just one material (3, in this case) are not shown.

For each property being compared, the top bar is ASTM A572 steel and the bottom bar is C97800 nickel silver.

Metric UnitsUS Customary Units

Mechanical Properties

Elastic (Young's, Tensile) Modulus, GPa 190
130
Elongation at Break, % 18 to 25
10
Poisson's Ratio 0.29
0.33
Shear Modulus, GPa 73
48
Tensile Strength: Ultimate (UTS), MPa 470 to 620
370
Tensile Strength: Yield (Proof), MPa 330 to 510
170

Thermal Properties

Latent Heat of Fusion, J/g 250
220
Maximum Temperature: Mechanical, °C 400
230
Melting Completion (Liquidus), °C 1460
1180
Melting Onset (Solidus), °C 1420
1140
Specific Heat Capacity, J/kg-K 470
390
Thermal Conductivity, W/m-K 51
25
Thermal Expansion, µm/m-K 13
16

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.2
4.0
Electrical Conductivity: Equal Weight (Specific), % IACS 8.2 to 8.3
4.1

Otherwise Unclassified Properties

Base Metal Price, % relative 2.0
40
Density, g/cm3 7.8
8.8
Embodied Carbon, kg CO2/kg material 1.6
5.1
Embodied Energy, MJ/kg 22
76
Embodied Water, L/kg 47
330

Common Calculations

Resilience: Ultimate (Unit Rupture Work), MJ/m3 100 to 110
31
Resilience: Unit (Modulus of Resilience), kJ/m3 290 to 690
120
Stiffness to Weight: Axial, points 13
8.1
Stiffness to Weight: Bending, points 24
19
Strength to Weight: Axial, points 17 to 22
12
Strength to Weight: Bending, points 17 to 21
13
Thermal Diffusivity, mm2/s 14
7.3
Thermal Shock Resistance, points 14 to 18
13