MakeItFrom.com
Menu (ESC)

ASTM A732 Cast Steel vs. ACI-ASTM CC50 Steel

Both ASTM A732 cast steel and ACI-ASTM CC50 steel are iron alloys. There are 25 material properties with values for both materials. Properties with values for just one material (7, in this case) are not shown.

For each property being compared, the top bar is ASTM A732 cast steel and the bottom bar is ACI-ASTM CC50 steel.

Metric UnitsUS Customary Units

Mechanical Properties

Brinell Hardness 140 to 440
210
Elastic (Young's, Tensile) Modulus, GPa 190
200
Poisson's Ratio 0.29
0.27
Shear Modulus, GPa 72 to 73
80
Tensile Strength: Ultimate (UTS), MPa 460 to 1470
430

Thermal Properties

Latent Heat of Fusion, J/g 250 to 260
300
Maximum Temperature: Mechanical, °C 400 to 430
1100
Melting Completion (Liquidus), °C 1440 to 1460
1420
Melting Onset (Solidus), °C 1400 to 1420
1370
Specific Heat Capacity, J/kg-K 470 to 480
490
Thermal Conductivity, W/m-K 39 to 50
17
Thermal Expansion, µm/m-K 13
11

Electrical Properties

Electrical Conductivity: Equal Volume, % IACS 7.1 to 7.7
2.3
Electrical Conductivity: Equal Weight (Specific), % IACS 8.2 to 8.9
2.7

Otherwise Unclassified Properties

Base Metal Price, % relative 2.0 to 3.8
14
Density, g/cm3 7.8 to 7.9
7.6
Embodied Carbon, kg CO2/kg material 1.4 to 1.7
2.7
Embodied Energy, MJ/kg 19 to 24
39
Embodied Water, L/kg 47 to 54
170

Common Calculations

Stiffness to Weight: Axial, points 13
15
Stiffness to Weight: Bending, points 24
26
Strength to Weight: Axial, points 16 to 52
16
Strength to Weight: Bending, points 17 to 37
17
Thermal Diffusivity, mm2/s 10 to 14
4.5
Thermal Shock Resistance, points 14 to 43
14