ASTM B522 Class II vs. 92-silver 8-tin-oxide
Both ASTM B522 class II and 92-silver 8-tin-oxide are otherwise unclassified metals. There are 6 material properties with values for both materials. Properties with values for just one material (17, in this case) are not shown.
For each property being compared, the top bar is ASTM B522 class II and the bottom bar is 92-silver 8-tin-oxide.
Metric UnitsUS Customary Units
Material Properties
Electrical Conductivity: Equal Volume, % IACS | 11 | |
76 to 80 |
Elongation at Break, % | 1.1 to 28 | |
32 to 34 |
Resilience: Ultimate (Unit Rupture Work), MJ/m3 | 4.4 to 63 | |
62 to 110 |
Shear Strength, MPa | 180 to 280 | |
150 to 210 |
Tensile Strength: Ultimate (UTS), MPa | 280 to 490 | |
230 to 320 |
Tensile Strength: Yield (Proof), MPa | 120 to 210 | |
120 to 300 |