Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 210 | |
120 |
Poisson's Ratio | 0.31 | |
0.32 |
Shear Modulus, GPa | 78 to 79 | |
45 |
Thermal Properties
Latent Heat of Fusion, J/g | 150 | |
200 |
Melting Completion (Liquidus), °C | 2460 to 2480 | |
1040 |
Specific Heat Capacity, J/kg-K | 170 | |
390 |
Thermal Conductivity, W/m-K | 450 | |
40 |
Thermal Expansion, µm/m-K | 12 | |
16 |
Electrical Properties
Electrical Conductivity: Equal Volume, % IACS | 50 to 53 | |
8.0 |
Electrical Conductivity: Equal Weight (Specific), % IACS | 32 to 34 | |
8.6 |
Otherwise Unclassified Properties
Density, g/cm3 | 14 | |
8.4 |
Embodied Carbon, kg CO2/kg material | 49 | |
3.6 |
Embodied Energy, MJ/kg | 760 | |
56 |
Common Calculations
Stiffness to Weight: Axial, points | 8.1 | |
7.8 |
Stiffness to Weight: Bending, points | 14 | |
19 |
Thermal Diffusivity, mm2/s | 190 | |
12 |