AWS E240 vs. ASTM A27 Cast Steel
Both AWS E240 and ASTM A27 cast steel are iron alloys. There are 22 material properties with values for both materials. Properties with values for just one material (9, in this case) are not shown.
For each property being compared, the top bar is AWS E240 and the bottom bar is ASTM A27 cast steel.
Metric UnitsUS Customary Units
Mechanical Properties
Elastic (Young's, Tensile) Modulus, GPa | 200 | |
190 |
Elongation at Break, % | 17 | |
25 to 27 |
Poisson's Ratio | 0.28 | |
0.29 |
Shear Modulus, GPa | 77 | |
73 |
Tensile Strength: Ultimate (UTS), MPa | 770 | |
460 to 550 |
Thermal Properties
Latent Heat of Fusion, J/g | 290 | |
250 |
Melting Completion (Liquidus), °C | 1390 | |
1460 |
Melting Onset (Solidus), °C | 1350 | |
1420 |
Specific Heat Capacity, J/kg-K | 480 | |
470 |
Thermal Conductivity, W/m-K | 15 | |
52 |
Thermal Expansion, µm/m-K | 15 | |
12 |
Otherwise Unclassified Properties
Base Metal Price, % relative | 14 | |
1.8 |
Density, g/cm3 | 7.7 | |
7.8 |
Embodied Carbon, kg CO2/kg material | 3.0 | |
1.4 |
Embodied Energy, MJ/kg | 42 | |
18 |
Embodied Water, L/kg | 160 | |
45 to 46 |
Common Calculations
Stiffness to Weight: Axial, points | 14 | |
13 |
Stiffness to Weight: Bending, points | 25 | |
24 |
Strength to Weight: Axial, points | 28 | |
16 to 20 |
Strength to Weight: Bending, points | 24 | |
17 to 19 |
Thermal Diffusivity, mm2/s | 3.9 | |
14 |
Thermal Shock Resistance, points | 19 | |
15 to 18 |